Indonesia
Film Faced Plywood
| Application | : | Film-Faced-Plywood-inner |
| Characteristics | : | Very flat | Up to 13 Times Repetition | Up to 13 Times Repetition | Excellent strength to weight ratio |
| Colour | : | Black (surface) |
| Material | : | Rubber wood | Phenolic film | Phenolic glue coating |
| Rubber Wood Characteristics | : | Can be used up to 13 times. Scratch resistant. Extremely durable. Very flat. High precision in Size. |
| Length | : | 2440 mm |
| Thickness | : | 12.0 mm | 15.0 mm | 18.0 mm | 21.0 mm | 30.0 mm |
| Width | : | 1220 mm |
| Bending | : | Long: MOE: 5000 - 5500 N/mm² ; MOR: 24 - 50 N/mm², Short: MOE: 4000 - 7000 N/mm² ; MOR: 20 - 65 N/mm² |
| Bonding | : | 0.7 N/mm² - 1.5 N/mm² |
| Concrete Casting Test | : | 13 Cycle (continued on) |
| Delamination | : | Passed |
| Density | : | < 14%, 650 - 750 kg/m3 |
| Determination of swelling in thickness | : | 5,83% |
| Emission | : | Classification F*** |
| Hardness | : | 6321.68 N |
| MC | : | 7,42% |
| Radial & Tangential Shrinkage | : | 2.05% & 0.24% |
| Stain Test | : | Passed |
| Water Resistant | : | Passed |
| Weather Test | : | 120 days (continued on) |
| Bending | : | JAS for Plywood 2014 |
| Bonding | : | JAS for Plywood 2014 |
| Concrete Casting Test | : | Internal Standard |
| Delamination | : | JAS for LVL 2013 Cyclic Extreme (Internal Standard) |
| Density | : | ASTM D143-94 2000 (Sec. 19) |
| Determination of swelling in thickness | : | BS EN 317 : 1993 |
| Emission | : | JAS for Plywood 2014 |
| Hardness | : | ASTM D 143 |
| MC | : | JAS for LVL 2013 |
| Radial & Tangential Shrinkage | : | ASTM D143-94 2000 (Sec. 20) |
| Stain Test | : | JAS for Plywood 2014 |
| Water Resistant | : | JAS for Plywood 2014 |
| Weather Test | : | JAS for Plywood 2014 |